Terrazzo in Pakistan: Chips Dana Floors, Tiles, Divider Strips and Cost
Terrazzo vs desi chips (dana) floors: in-situ vs tile, grinding stages, brass and glass strips, PKR per sq ft and care in Pakistan. Get a free quote.
Captivating Marble Design Team · · Updated · 19 min read

Key takeaways
- A chips (dana) floor is cement-based terrazzo: crushed marble chips in white or grey cement, ground flat and polished on site.
- Our Chips Dana costs PKR 180–420 per sq ft laid, ground and polished (November 2026), the cheapest stone surface we supply.
- Pre-cast chips tiles are 24 x 24 inches and suit occupied houses and upper floors; large open areas are cheaper poured in place.
- Crews usually wait about a week before the first grind, so a small poured floor takes one to two weeks from pour to polish.
- Brass strips cost most and polish to a gold line; glass is the traditional low-cost choice but can chip during grinding.
The short answer
Terrazzo is a floor of marble chips set in a binder, usually cement, ground flat and polished so the chips show as a speckle. In Pakistan it is called a chips or dana floor (dana means grain), poured in place between divider strips or laid as pre-cast tiles. Our Chips Dana costs PKR 180 to 420 per square foot, laid and polished.
The classic desi version is poured over a concrete base, divided into panels by brass, glass or aluminium strips and ground smooth on site; the tile version is pressed and ground in a workshop, laid like any other tile and ground again once fixed. Either way it is the least expensive stone surface we supply.
This guide explains how a chips floor differs from imported resin systems, when to pour in place and when to use tiles, what happens at each grinding stage, how to choose divider strips, what moves the price, and how to look after the floor in Pakistani heat, dust, hard water and monsoon damp.
Chips Dana figures are our current quote range per square foot, laid, ground and polished (November 2026). Any other figure in this post is an indicative market range and is labelled as such. Confirm the final rate against a written quotation for your site.
What is a chips floor made of?
A chips floor is made of crushed marble aggregate, a white or grey cement binder, divider strips and a sound concrete base. The idea is old and simple. Italian builders in the Venetian region used marble offcuts that were too small for anything else, set them in a lime or cement bed, and rubbed the surface flat with stones. The word itself comes from the Italian for terrace, because these were the floors of terraces and courtyards. The method travelled across the world in the twentieth century, and in South Asia it became the standard finish for verandas, school corridors, hospital wards and the speckled drawing-room floors that many older houses in Lahore, Rawalpindi and Karachi still have.
Every chips floor, whatever it is called, has the same four parts:
- Aggregate. Crushed marble in graded sizes. In our workshop this comes from offcuts of Pakistani marble, so the colours available are the colours of local stone: white, cream, grey, black, green, red and yellow. See our glossary entry on Chips Dana for the short definition.
- Binder. White cement for clean, bright mixes; grey cement for darker or more economical ones. Mineral pigment can tint the binder so the background colour matches or contrasts with the chips.
- Divider strips. Thin metal, glass or plastic strips set on edge to split the floor into panels. They control cracking and let you pour colours side by side.
- Base. A sound, level concrete slab and a bedding screed. Most chips-floor failures start here, not in the surface.
Cement-based or resin-based
Abroad, many new commercial floors use an epoxy (resin) binder instead of cement. Resin systems are laid much thinner, cure in a day or two, come in strong colours and can carry glass, shell or mirror aggregate. They also need a specialist contractor, a very dry and flat base, and a far higher budget. We do not supply resin systems; everything in this guide refers to the cement-based chips floor that is standard in Pakistan, which is what our Chips Dana is. Our guide to epoxy floors compared with marble covers the cost and care trade-offs.
Chip size and mix
Chip size sets the character. Fine chips, roughly the size of rice grains, give a quiet surface that reads almost as one colour from standing height. Medium chips give the familiar speckle. Coarse chips, close to fingernail size or larger, give a bold, almost mosaic look and need more grinding to open up. Many mixes blend two sizes so the small chips fill the gaps between the large ones and less binder shows. Ask to see a ground and polished sample of the exact mix before work starts, because a wet bucket of chips looks nothing like the finished floor.
In-situ chips floor or terrazzo tile?
Pour in place for large, open, empty areas; choose pre-cast 24 x 24 inch tiles for occupied houses, upper floors and room-by-room work. You can have a chips floor two ways. In-situ (cast in place) means the mix is spread over the base inside a grid of strips, compacted, cured and ground on the spot. Pre-cast tile means the chips and cement are pressed into tiles in a workshop, cured and given a first grind there, then fixed on site with mortar or adhesive and ground again so the joints sit flush. We supply pre-cast tiles at 24 x 24 inches where pouring on site is impractical.
| Point | In-situ (poured on site) | Pre-cast tile |
|---|---|---|
| Look | Jointless panels; strips are the only lines | Tile joints every 24 in, plus any strips |
| Site time | Longest: pour, wet cure, several grinds | Shorter: fix, short cure, one site grind |
| Mess and water | Heavy slurry on site for days | Less, but the final grind is still wet work |
| Best for | Large open areas, porches, courtyards, corridors, stairs cast in place | Occupied houses, upper floors, small rooms, phased work |
| Colour control | Mixed on site; batch-to-batch care needed | Made in one batch; easier to keep consistent |
| Repairs | Patch with the same mix and regrind | Lift and replace a tile, then regrind the area |
| Patterns | Any shape the strips can follow, including curves | Square grid; borders cut from tile or added in slab |
As a rule of thumb, pour in place when the area is large, open and empty, and you can live with a week or more of wet work. Choose tiles when people are living in the house, when the floor is upstairs and slurry would run through the building, or when you are doing one room at a time. Either way the finished surface is ground, polished and sealed on site, so both need a grinding machine, water and a skilled operator.
How a cast-in-place chips floor is laid
Good chips floors look simple because the work is done in the right order and nothing is rushed. This is the sequence a competent crew follows; use it to check a contractor's method statement.
- Check the base. The concrete slab should be fully cured, sound, clean and close to level. On a ground floor there must be a damp-proof course or membrane underneath, or monsoon damp will rise through the floor and leave white salt marks.
- Lay the bedding screed. A sand-cement screed brings the base to the right height and fall. Outdoors and in wet rooms it should slope gently to a drain.
- Set the strips. Strips are fixed on edge in mortar along chalk lines, at the finished-floor height, forming the panel grid or pattern. Their tops become the level guide for the surface.
- Place the mix. The chips-and-cement mix is spread into one panel at a time, compacted and rolled or tamped so the chips pack tightly, with extra chips scattered and pressed in where the surface looks thin.
- Wet cure. The surface is kept damp, usually under wet hessian or by regular sprinkling, so the cement gains strength slowly. Curing that dries too fast causes shrinkage cracks.
- First grind. Once the surface is hard enough that chips no longer pull out, a coarse grinding stone or diamond tooling is run over it wet to cut back the cement skin and expose the chips.
- Grout (slurry) coat. The first grind opens small pinholes and voids. A cement slurry in the same colour as the binder is worked into them and left to cure.
- Further grinds. Progressively finer stones or pads remove the slurry film, flatten the strips with the surface and close the scratches left by the coarse grit.
- Polish and seal. The final fine passes bring up the shine, the floor is washed and dried, and a penetrating sealer is applied.
Crews commonly wait around a week before the first grind, longer in a cold Lahore or Islamabad winter, and allow further days between grout and the later grinds. A small floor therefore takes one to two weeks from pour to polish, and a large one longer. If someone offers to pour on Monday and hand over a polished floor on Thursday, ask how the cement will have cured.
Grinding and polishing: where the quality is made
Grinding, called ragrai on Pakistani sites, is what turns a rough cement surface into a floor you can see your reflection in. It is also where a cheap job usually falls short. The aim is to cut the surface down evenly until the chips are exposed across their widest section, with the strips and the binder flush around them.
Coarse, medium and fine
- Coarse grits remove the cement skin and bring strips and chips to one plane. Too little coarse grinding leaves chips that look like dots instead of stones; too much wastes the surface.
- Medium grits take out the deep scratches from the coarse stage. Skip them and the floor will look polished but show swirl marks in side light.
- Fine grits and polishing pads close the surface and bring up the gloss. The more fine stages, the deeper the shine.
Machines on local sites range from heavy single-disc ragrai machines fitted with grinding stones to newer planetary grinders with diamond tooling. Both can produce a good floor. What matters more is that the operator works wet, overlaps passes, keeps the machine moving at the edges and does not jump grits. Corners, skirting junctions and stair nosings are finished with a hand grinder, so ask who does them and how.
Old-style acid polishing
Some older polishers finish chips floors by rubbing in oxalic acid powder with a stone or pad, which gives a quick gloss. It works by reacting with the calcite in the marble chips and the surface of the cement, so used heavily or on the wrong stone it can dull or roughen the very surface it is meant to shine. Modern practice is to build the gloss mechanically through finer diamond pads and then seal. If acid will be used, ask for it to be neutralised and rinsed thoroughly before any sealer goes on.
Dust, slurry and protection
Wet grinding produces a grey slurry that stains timber, paint and fresh plaster. Doors, skirting, kitchen units and stair balusters should be fitted after grinding or masked with plastic and tape. The slurry should be collected and taken off site, not washed into drains, where it sets like cement. Our guide to marble polishing in Pakistan covers machines, grits and indicative polishing rates in more depth.
Which divider strips are best: brass, glass, aluminium or PVC?
Brass is best for a main room that should last, glass for low-cost verandas and utility areas, aluminium for modern grey mixes and PVC for tight budgets or curves. Strips do two jobs. First, they split the floor into smaller panels so the cement can shrink as it cures without cracking at random; any crack that does form tends to run along a strip, where it is hidden. Second, they are a design tool: they set out borders, grids, diagonals, medallions and colour changes, and their colour and width become part of the pattern.
| Strip | Look | Strengths | Watch for |
|---|---|---|---|
| Brass | Gold line that polishes with the floor | Durable, classic, suits white and cream mixes; reads as a deliberate design line | Costs the most; darkens over time unless re-polished; must be ground flush, not left proud |
| Glass | Thin green-tinted or clear line | Very low cost; traditional on South Asian chips floors; does not tarnish | Edges can chip during grinding or under heavy furniture; hard to replace neatly |
| Aluminium | Silver-grey line | Cheaper than brass, crisp modern look on grey mixes | Softer metal; reacts with fresh wet cement and can corrode in constantly wet areas |
| PVC / plastic | Black, white or coloured line | Cheapest; flexible for curves; can match or contrast the binder | Scuffs and can lift at edges; less crisp after years of traffic |
Panel size and layout
Crews generally keep cement panels to roughly 3 to 4 feet square, smaller in very hot or exposed areas such as rooftops and car porches, because smaller panels have less shrinkage to absorb. Plan the grid from the centre of the room so cut panels at the walls are even on both sides, line strips up with door openings, and put a strip wherever the floor changes colour or meets a different material. On a long corridor, a strip across the width every few feet looks tidier than a square grid.
Strips also make it easy to combine a chips field with a coloured marble border. A band of Design Patti inlay around the edge of a room, or a black or green marble strip at the threshold, lifts a plain floor without changing the main material.
What a chips floor costs
Our Chips Dana quote range is PKR 180 to 420 per square foot as of November 2026, laid, ground and polished. The figure for your floor depends on choices you make and on the site. The product page has the current Chips Dana price per square foot; the points below explain where in the range a job will land.
- Chip colour and source. Plain white or grey chips are the cheapest; selected colours, mixed colours and black or green chips cost more.
- White or grey cement. White cement and pigments raise material cost but give cleaner colours.
- Strip material. Glass and PVC are cheapest, aluminium sits in the middle, brass costs the most. Strip choice and grid size are listed separately on our quote.
- Pattern. A plain grid is quick to set out; curves, medallions, borders and multi-colour panels take far more labour.
- In-situ or tile. Tiles can save site days on small or occupied jobs; large open areas are usually more economical poured in place.
- Area and access. Small jobs carry a minimum charge for machines and crew; upper floors and narrow access add handling.
- Base condition. Breaking out an old floor, levelling a poor slab or adding a damp-proof layer is extra work before the chips go down.
Worked examples at our range
| Job | Area | Estimated cost (PKR) |
|---|---|---|
| Hallway, 15 x 6 ft | 90 sq ft | 16,200 – 37,800 |
| Car porch, 20 x 15 ft | 300 sq ft | 54,000 – 126,000 |
| Veranda and courtyard, 25 x 16 ft | 400 sq ft | 72,000 – 168,000 |
| Rooms and passages on one house floor | About 900 sq ft | 162,000 – 378,000 |
To run your own figures, measure each room in feet, multiply length by width and use our stone cost estimator. For a poured floor wastage is small; for pre-cast tiles allow about 5 to 10% for cuts at the walls.
How it compares with slab marble
For context, our most economical slab whites are China White at PKR 450 to 800 and Medium White at PKR 550 to 950 per square foot. A chips floor is therefore the cheapest way to get a real marble surface across a large area, and it has no slab joints to line up. Our marble vs tiles guide sets chips against porcelain and ceramic over twenty years. What it gives up is the calm, continuous look of a single stone; a speckled floor reads busier, especially with coarse chips.
We do not supply epoxy (resin) terrazzo, glass-aggregate mixes or pre-cast worktops and stair treads in a resin binder, so we do not quote rates for them here. They are specialist products priced per job; ask a resin flooring contractor for a written rate if you want that look.
Where chips floors work, and where to think twice
Good places for it
- Car porches and driveways under cover. Hard-wearing, repairable and jointless. Use a honed or lightly ground finish outdoors for grip.
- Verandas, courtyards and rooftops. Cheap per square foot over large areas. Keep panels small and the slope to drains correct.
- Stairs. Treads and risers can be cast in place with a contrasting nosing strip, or made from pre-cast pieces.
- Corridors, schools, clinics and offices. The reason so many public buildings in Punjab use it: it takes heavy foot traffic and can be reground rather than replaced.
- Kitchens and utility rooms (floors). It shrugs off dropped pans better than thin tile and has no grout lines to blacken.
- Retro and modern interiors. A white-cement mix with fine white and grey chips and brass strips looks contemporary; coloured coarse chips give the classic 1970s floor.
Where to be careful
- Wet bathrooms and poolsides. A high polish is slippery when wet. Use a honed finish and slope the floor properly.
- Sun-baked open roofs. Strong summer heat and rain cycles move the surface. Small panels, good curing and a sealer are essential; expect some hairline cracking over time.
- Floors over timber or weak slabs. Any movement in the base shows as cracks. Fix the structure first.
- Rooms where you want a calm, continuous look. Choose slab marble instead, such as Medium White or Ziarat White.
For more ideas on combining chips with borders, medallions and slab stone, see our marble floor design guide, and browse flooring and wall tile for the slab and tile stones we supply.
Pakistani conditions: heat, monsoon, dust and hard water
Cement-based floors are sensitive to the weather while they cure and to the way they are cleaned for the rest of their lives. A few local precautions make a large difference.
- Summer heat. In May to July, pour early in the morning, shade the area and keep it wet. Fast drying is the main cause of shrinkage cracks across panels.
- Winter cold. In northern cities, cement gains strength slowly in cold weather, so grinding starts later. Do not grind a floor that is still green just to keep to a date.
- Monsoon damp. On ground floors without a damp-proof layer, moisture rises through the slab and carries salts to the surface as white powder (efflorescence). Fix the damp before laying, and let new floors dry before sealing.
- Dust. Fine dust and grit act like sandpaper on a polished surface. Put mats at every outside door and dry-mop daily.
- Hard water. Mineral-rich water leaves white marks as it dries. Wipe up standing water and avoid letting buckets of hard water sit on the floor.
Care, sealing and restoring an old chips floor
Daily and weekly care
- Dry-mop or vacuum daily, then wash with plain water or a pH-neutral stone cleaner.
- Avoid acid toilet and tile cleaners, vinegar and lemon. Acid attacks both the marble chips and the cement around them.
- Avoid strong bleach and caustic cleaners used neat; they weaken the cement binder over time.
- Put felt pads under chairs and tables, and lift rather than drag heavy furniture.
Sealing
A chips floor is porous, and the cement binder is more absorbent than the marble chips. Seal it with a penetrating sealer after the final polish and reseal every couple of years in heavy traffic, or sooner in kitchens and porches where oil and tyre marks are common. To check whether it needs resealing, drip a little water on the busiest area: if it darkens the surface within a few minutes instead of beading, it is time.
Bringing an old floor back
One of the best things about chips floors is that a dull, scratched floor from decades ago can usually be restored rather than replaced. The surface is reground with coarse grits to remove wear, cracks and chipped areas are cut out and patched with a matching mix, missing or loose strips are reset, and the floor is then taken through the medium and fine grits, polished and sealed. Colour matching a patch is never perfect on an old floor, so ask to see a test patch before the whole area is done. Where an old floor has hollow, drummy areas, the bedding has failed and those panels need to be broken out and relaid.
Questions to ask before you hire a crew
- Can I see a ground and polished sample of this exact mix, chip size and cement colour?
- What strip material, gauge and panel size will you use, and is it priced in the rate?
- How will the base be prepared, and is there a damp-proof layer on the ground floor?
- How long will you wet cure before the first grind, and how many grinding stages are included?
- Who finishes edges, corners and stair nosings, and with what tool?
- Is sealing included, and which sealer will you use?
- How will slurry be collected and removed, and what will you protect?
- Is the rate per square foot of finished floor, and are skirting, steps and borders priced separately?
We cover the full fitting process, from measurement to handover, on our stone installation page. If you want to see the chips and colours in your own light first, order from our samples page.
Get a quote for a chips floor
Send us the room sizes, a photo of the existing floor and whether you want it poured in place or laid as tile, along with your preferred chip colour and strip type. We will come back with a free written quote that lists base work, mix, strips, grinding stages and sealing line by line, with lead times for your city.
Written by
The Captivating Marble Design Team
Fabricators, templaters and stone designers
We template, cut and install natural stone every day and write about what we learn — pricing, layouts, care and the mistakes we help clients avoid.
Book a free design consultation